TECHNET Archives

February 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Douglas Pauls <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 11 Feb 2013 07:23:26 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (136 lines)
Inge,
Iowa has corn and soybeans.  Idaho has the potatos.......

Doug Pauls



From:   Inge Hernefjord <[log in to unmask]>
To:     <[log in to unmask]>
Date:   02/11/2013 05:21 AM
Subject:        Re: [TN] Anti-splashing solder wire [NTC]
Sent by:        TechNet <[log in to unmask]>



Thanks Pat! WHAT a place! Breathtaking!  More superlatives!
On the BR2 star engine: How on earth can you fix the enormous centrifugal
forces? Whole engine rotates! Unbelievable! And still more
make-me-just-gasp: how in the name of Iowa's potatoes do you make the
interface for accelerator (throttle ) and fuel???

Thanks again! Had no idea there was such a museum. Models museums are many
but models with full functions, that's something else!

Inge

On 11 February 2013 11:08, Goodyear, Patrick <[log in to unmask]> wrote:

> Modeling!
>
> Check out the http://www.craftsmanshipmuseum.com on the internet.  Those
> guys make me very humble.
>
> Everything one could imagine in miniature and most if not all of it 
FULLY
> functional.
>
> I have spent hours browsing that site, on my bucket list to go visit the
> museum.
>
> Pat
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
> Sent: Sunday, February 10, 2013 8:31 AM
> To: [log in to unmask]
> Subject: Re: [TN] Anti-splashing solder wire [NTC]
>
> Well thank you Inge.
> I built a very accurate Porsche model which I was given for a project
> whilst convalescing some years ago. It took me about 5 months at a 
couple
> of hours a week. I half expected it to fire up when I finished it.
> Presently I am making a Christmas present of a Triumph TR4. This is more 
of
> a child's toy.
> I can confirm though its realism in one area: fitting the body parts - 
it
> needs bending and fettling just like a real one. I will put a scale oil
> puddle under it to make it authentic.
>
> Best Wishes
>
>
>
> Mike
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord
> Sent: Sunday, February 10, 2013 12:57 PM
> To: [log in to unmask]
> Subject: Re: [TN] Anti-splashing solder wire
>
> Mike, former Indium star, gave me a short but covering lesson about 
solder
> wires, so good that I honored him in Dropbox under ' Comments from 
members'
> . I will drop unusally short,  concentrated and clever comments there. 
Who
> will be next?
>
>
> > Inge
> >
> > PS. NTC q: has anyone seen or built such a one
> >
>
>
> > http://www.rcarmory.com/kit_tiger1.html#description
> >
> >
> >
> >
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud 
service.
> For more information please contact helpdesk at x2960 or 
[log in to unmask]
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud 
service.
> For more information please contact helpdesk at x2960 or 
[log in to unmask]
> ______________________________________________________________________
>
>
> PG&E is committed to protecting our customers' privacy.
> To learn more, please visit
> http://www.pge.com/about/company/privacy/customer/
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud 
service.
> For more information please contact helpdesk at x2960 or 
[log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2