     If this is referring to press fit connector holes, our vendor 
     tolerances are +/- .001 on the copper plating and +/- .002 on the 
     solder plating. We have had problems in the past with Board 
     Manufactures exceeding these tolerances and the Press Fit connectors 
     are very hard to install.
        If not "Never Mind"
     
     ERic Bernal
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: Press fit padstacks
Author:  [log in to unmask] at ~INTERNET
Date:    7/27/95 3:03 PM


Received: by ccmail
Received:  from netcomsv by pragma.com (UUPC/extended 1.11) with UUCP;
           Thu, 27 Jul 1995 15:02:33 PDT
Received: from miso.wwa.com by netcomsv.netcom.com with SMTP (8.6.12/SMI-4.1)
    id OAA10881; Thu, 27 Jul 1995 14:32:22 -0700
Resent-Date: Thu, 27 Jul 1995 14:32:22 -0700 
Received: from ipc by miso.wwa.com with uucp
    (Smail3.1.28.1 #8) id m0sbaZB-000FRDC; Thu, 27 Jul 95 16:34 CDT
Received: by ipchq.com (Smail3.1.28.1 #2)
    id m0sbZyV-0000GsC; Thu, 27 Jul 95 15:56 CDT
Old-Return-Path: <miso!starman.convex.com!ondricek> 
Date: Thu, 27 Jul 95 15:44:57 -0500
From: [log in to unmask] (Doug Ondricek) 
X-ccAdmin: postmaster@netcomsv
Message-Id: <[log in to unmask]> 
To: [log in to unmask]
Subject: Press fit padstacks
Resent-Message-ID: <"x23x-1.0.e16.Zr_5m"@ipc> 
Resent-From: [log in to unmask]
X-ccAdmin: postmaster@netcomsv
X-Mailing-List: <[log in to unmask]> archive/latest/752 
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]
     
I'd like to get some feedback on what other people are using for pad and 
antipad sizes relative to finished hole size on press fit holes.
     