Thieving is nothing more than added copper (usually in a specific pattern,
crosshatch, dots, etc) in non-functional areas of the board, applied for the
purpose of providing a more uniform surface area during electroplating.
Common uses are where there are long isolated traces leaving areas of more
dense copper features.
Was that laymen?
Franklin
----- Original Message -----
From: "Phil Nutting" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, July 22, 2005 1:34 PM
Subject: [TN] layman's definition of theiving
Ok, I have to admit my lack of knowledge.
Can someone point me to a the Cliff's Notes version of Theiving on PC
boards?
Thanks in advance.
Phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|