TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Date:
Thu, 27 May 2010 15:05:56 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Rex Waygood <[log in to unmask]>
Subject:
From:
Rex Waygood <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (89 lines)
Sensible hygiene should be adequate.
I would consider each item at a time and decide to share or not.
It would depend upon the cost of the items and the difficulty in cleaning, i.e. we don't share tools between waves, they are cheap but hard to clean. 
We have swapped wave pallets where the product has switched but ensured they were clean, wave pallets are expensive but easy to clean and the bath capacity would mean a large amount of solder would be required to produce a measureable cross contamination.
Stencils we have moved across but not many, tools at print are shared but easy to clean.
You are not looking for zero lead, you are looking to comply. Note lead free solders are not lead free so your margin is reduced.
OK?
Rex


Rex Waygood
Technical Manager
 
Hansatech EMS provides value manufacturing through engineering and quality
 
Hansatech EMS Limited
Benson Road
Nuffield Industrial Estate
Poole
Dorset
BH17 0RY
 
+44 (0)1202 338200


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: 27 May 2010 14:39
To: [log in to unmask]
Subject: [TN] Cross contamination of RoHS boards

Dear Technos,

 

Did anyone perform contamination testing of RoHS boards? I mean, we would like to have hard evidence telling where to draw the line: can we re-use SnPb stencils for RoHS, can we use the same cutters, picks , crimpers, lead forming dies, press-fit tooling, wave pallets, etc? I know the "better safe than sorry" policy is the best, but at times scrapping all the tooling sets for a product becomes very expensive!

 

Are there any reports, even pay ones, dealing with this topic?

 

Thanks,

 

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer T | 450.967.7100 ext.244 E | [log in to unmask] <mailto:[log in to unmask]> W | www.digico.cc <http://www.digico.cc/> 

 
 N'imprimer que si nécessaire - Print only if you must

 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2