text/plain (54 lines)
MSD's need baking only if they have exceeded their exposure limits.
We use a McDry for Reeled parts.
Periodically, we need to remove the parts from T+R, bake, then put them
in tubes or trays.

The best thing to do is control the exposure time if possible.

-Carrie 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Marsico, James
Sent: Tuesday, April 20, 2004 4:20 PM
To: [log in to unmask]
Subject: [TN] Moisture sensitive Components

Good Day Technet:
Being a military OEM, we've never had to use plastic components but
we're just starting to use them.  I'm embarrassed by the amateurish
nature of this question, but I have no one else to turn to, so here
goes...  I know that moisture-sensitive components require baking prior
to reflow, but how do you bake components that are supplied in tape and
reel?  Can the tape and reels be baked along with the components or do
you have to remove the parts and re-package after baking?

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2