TECHNET Archives

January 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Wed, 18 Jan 2012 14:55:59 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Graham Naisbitt <[log in to unmask]>
Message-ID:
Subject:
From:
Graham Naisbitt <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
<000401ccd5e3$d1a9a430$74fcec90$@com>
MIME-Version:
1.0 (Apple Message framework v1251.1)
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (210 lines)
Thanks Steve - and if they do, send them to me.

Graham

On 18 Jan 2012, at 13:19, Steve Gregory wrote:

> Hi Graham,
> 
> I've got it posted on my page now, it's at:
> 
> http://stevezeva.homestead.com/SG_PCT01_LR.pdf
> 
> I hope nobody pings me about copyrights again...  :o)
> 
> Steve
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Naisbitt
> Sent: Tuesday, January 17, 2012 10:42 AM
> To: [log in to unmask]
> Subject: Re: [TN] Expired Solder Paste
> 
> Hi Doug
> 
> Already done. Steve, do please feel free to post it as Doug suggests.
> 
> Graham
> 
> On 17 Jan 2012, at 13:48, Douglas Pauls wrote:
> 
>> Perhaps Graham, if you can provide the document to Steve Gregory to post, 
>> or post it on the Gen3 web site, it would be a convenient place for many 
>> to get the document you reference.
>> 
>> Doug Pauls
>> 
>> 
>> 
>> Graham Naisbitt <[log in to unmask]> 
>> Sent by: TechNet <[log in to unmask]>
>> 01/17/2012 06:03 AM
>> Please respond to
>> TechNet E-Mail Forum <[log in to unmask]>; Please respond to
>> Graham Naisbitt <[log in to unmask]>
>> 
>> 
>> To
>> <[log in to unmask]>
>> cc
>> 
>> Subject
>> Re: [TN] Expired Solder Paste
>> 
>> 
>> 
>> 
>> 
>> 
>> Hi Juliano and fellow Techies,
>> 
>> It might be useful to you to consider using a relatively new Process 
>> Control Standard available from SMART Group (www.smartgroup.org) entitled:
> 
>> Control of Solder Paste used in Electronic Assembly Process
>> This was developed from the IPC-J-STD005 solder paste test methods, but 
>> adapted for use by folks using paste as opposed to the manufacturer.
>> 
>> The Scope states:
>> This Standard is intended to determine the suitability of solder paste 
>> prior to its employment on the production line; reduce process defects and
> 
>> minimise rework.
>> The tests are, by necessity, fast and simple to perform; with commercially
> 
>> available equipment and may be completed in less than 1 hour.
>> A list of defects, test methods and the time/cost implications are shown 
>> 
>> If anyone would like a copy they could contact SMART Group or let me know 
>> and I can forward a copy. 
>> 
>> Graham Naisbitt
>> Gen3 Systems Limited
>> www.gen3systems.com
>> [log in to unmask]
>> On 16 Jan 2012, at 13:29, Juliano Pacheco wrote:
>> 
>> 
>>> Hi,
>>> 
>>> What are the consequences of using expired solder paste?
>>> How long after the expired date is "acceptable"?
>>> 
>>> Thank you.
>>> 
>>> Juliano Pacheco
>>> 
>>> 
>>> ______________________________________________________________________
>>> This email has been scanned by the Symantec Email Security.cloud 
>> service.
>>> For more information please contact helpdesk at x2960 or 
>> [log in to unmask] 
>>> ______________________________________________________________________
>>> 
>>> ---------------------------------------------------
>>> Technet Mail List provided as a service by IPC using LISTSERV 16.0
>>> To unsubscribe, send a message to [log in to unmask] with following text 
>> in
>>> the BODY (NOT the subject field): SIGNOFF Technet
>>> To temporarily halt or (re-start) delivery of Technet send e-mail to 
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>> To receive ONE mailing per day of all the posts: send e-mail to 
>> [log in to unmask]: SET Technet Digest
>>> Search the archives of previous posts at: 
>> http://listserv.ipc.org/archives
>>> For additional information, or contact Keach Sasamori at [log in to unmask] 
>> or 847-615-7100 ext.2815
>>> -----------------------------------------------------
>> 
>> 
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask] 
>> ______________________________________________________________________
>> 
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 16.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to 
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to 
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at: http://listserv.ipc.org/archives
>> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 
>> 847-615-7100 ext.2815
>> -----------------------------------------------------
>> 
>> 
>> 
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask] 
>> ______________________________________________________________________
>> 
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 16.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at: http://listserv.ipc.org/archives
>> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
>> -----------------------------------------------------
> 
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2