It is now possible to AOI Double Treat with a Gerber AOI which uses a near
infrared reflective light source.
George Murray
>----------
>
>Scott;
>
>Double treat is worth looking at. however, you can't AOI it. This is
probably
>the biggest drawback.
>
>Gary Ferrari
>
***************************************************************************