TECHNET Archives

April 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Date:
Tue, 1 Apr 2003 23:34:18 +0300
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii; format=flowed
From:
Brian Ellis <[log in to unmask]>
Parts/Attachments:
text/plain (51 lines)
I agree, but it even goes farther than that. Some activators may be
nearly neutral, such as amine hydrochlorides. These decompose at close
to soldering temps, to release highly acidic gases, which would not be
seen independently as acids during a KOH titration.

Brian

Rudy Sedlak wrote:
> Siggi:
>
> What a great question, because it cuts to the heart of the issue.
> Unfortunately, it cannot be answered, for many reasons, not the least
> being that there is no absolute definition of any of the fluxes, they
> are defined by the vendors, who each have a slightly different concept
> of what is needed for a particular kind of flux.
>
> But, more, the difference between fluxes is less the amount of acid,
> than the strength of the acid being used.  The rosin acids are very
> weak, and on the other end of the scale, some fluxes may even contain
> strong mineral acids like Hydrochloric, and Hydrobromic.
>
> So, the mg KOH/gram is a meaningless number.
>
> Great question.
>
> Rudy Sedlak
> RD Chemical Company---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2