TECHNET Archives

October 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Ioan Tempea <[log in to unmask]>
Date:
Fri, 21 Oct 2011 17:46:43 -0400
Message-ID:
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Vladimir Igoshev. PhD" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Subject:
From:
"Vladimir Igoshev. PhD" <[log in to unmask]>
X-cc:
In-Reply-To:
Organization:
SENTEC Testing laboratory Inc.
MIME-Version:
1.0
Parts/Attachments:
text/plain (35 lines)
Hi Ioan,

  
I'd say it's too much discoloration for a thin organic film on top of
Au. It looks like something else.Do you have appropriate planar SEM
taken from the areas? I wouldn't expect to see anything in
cross-section.
-- 
Best regards,

Vladimir Igoshev. PhD                          mailto:[log in to unmask]

SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2