Stella,
IPC-A-610B, Paragraph 4.1, defines as a nonconforming defect for all
classes:
Solder balls/splashes violate minimum electrical design clearance, or
are not entrapped in a permanent coating or attached to a metal contact.
Nonconforming process indicators for all classes are:
- Solder balls/splashes which are within 0.13mm of lands or traces, or
exceed 0.13mm in diameter.
- More than five (5) solder balls/splashes (0.13mm or less) per 600
mm2.
Note: Entrapped is intended to mean normal service environment of the
product will not cause a solder ball to become dislodged.
Hope this helps.
Mary Muller
Materials and Processes
ELDEC Corp.
Lynnwood, WA
> ----------
> From: [log in to unmask][SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;[log in to unmask]
> Sent: Thursday, February 26, 1998 12:50 PM
> To: [log in to unmask]
> Subject: [TN] Solder balls spec
>
> Dear colleagues:
> Sorry, but I have to return to the solder balls spec. issue.
> I know, that IPC-S-815B ( 3.6.6) had the criteria for the solder
> balls (
> less than 0.005", no more than 5 per one sq. inch).
>
> Now, IPC-S-815 was replaced by J-STD-001. But , I can not find any
> solder
> balls spec in J -STD.
>
> We are NoClean chemistry users, and will always have tiny solder
> balls,
> although we are trying to reduce its number.
>
> I need an official document to accept presence of the solder balls up
> to
> the certain level, of course.
> Please, help!!
> Stella Neyman
> Eaton Co.
> 248-608-7289
> E-mail: [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|