TECHNET Archives

January 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 5 Jan 2010 17:12:19 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="ISO-8859-1"
From:
Joe Fjelstad <[log in to unmask]>
Parts/Attachments:
text/plain (71 lines)
Hi Steve
 
Your question brings up questions.  Are the bonds, which are being  tested 
and failing, stitch or ball? Can you notice any physical differences in  the 
failures? Also what type of nickel plating are you using? It might be  that 
a higher stressed nickel is fracturing in bonding and setting up  the site 
to fail. 
 
Cheers,
Joe    
 
 
In a message dated 1/5/2010 1:18:08 P.M. Pacific Standard Time,  
[log in to unmask] writes:

Hi  All,

I have a wire bond question to the wire bond gurus who have helped  me out 
a lot in the past. Made 2 versions of a flex circuit - only varied the  
nickel thickness. Application is thermosonic gold wire bonding.

Flex  circuit lead is .0032 wide - version 1 - nickel is 150 microinches - 
soft gold  is 50 microinches- pull strength is X

Version 2 - nickel is 40 microinches - soft gold is 50  microinches - pull 
strength is approx. ½X  of version 1-

Is this  what I should expect?



Regards Steve Kelly



Steve  Kelly (PLEASE NOTE NEW E-MAIL ADDRESS)

(416) 750-8433  (work)

(416) 750-0016 (fax)

(416) 577-8433  (cell)




---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To  receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]:  SET Technet Digest
Search the archives of previous posts at:  http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information,  or contact Keach Sasamori at [log in to unmask] or 
847-615-7100  ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2