TECHNET Archives

July 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 8 Jul 2009 10:33:12 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
Victor Hernandez <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (235 lines)
Just to be clear, this application is for an edge connector,
card/board/PWB/PCB, gold finger contact mating surface and not a
solderable interface.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob METCALF
Sent: Wednesday, July 08, 2009 10:10 AM
To: [log in to unmask]
Subject: Re: [TN] Electroless Nickel Electroless Palladium Immersion
Gold (ENEPIG)

Just a comment on the cost of ENEPIG. Using palladium after nickel and 
before gold, limits the gold deposition to normally about two
microinches 
as opposed to about four microinches in normal ENIG. If you look at
metal 
pricing, palladium is currently selling for about $230 per oz and gold
is 
selling for about $920 per oz. The ENEPIG process averages about 5 
microinches of palladium. By the self limiting nature of the palladium 
with the gold you are saving around 2 microinches of gold (at $920 per
oz) 
and replacing it with 5 microinches of palladium (at $230 per oz) the
cost 
difference is very small, in fact I have talked to some manufactures
using 
this process and they have stated the process cost less.

I believe the perception of the high cost is from the late 90's early
2000 
when palladium went as high as $1300 per oz. ENEPIG was gaining
popularity 
in the late 90's when the price of palladium went through the roof. 
Because of the huge impact of the palladium, it effectively killed this 
process. In recent years with the cost of palladium stabilizing back
down 
to reasonable levels, we are seeing increased interest in this process.

With cost no longer a factor and the enormous benefits using palladium 
between the nickel and gold layer, I expect you are going to see 
significant growth in this process.

Regards,

Bob Metcalf
Atotech Western Regional Manager

Cell 714-334-7667
E-Mail [log in to unmask] 

This e-mail and any attachments hereto are business documents of Atotech

USA Inc. and may contain CONFIDENTIAL OR PROPRIETARY BUSINESS
INFORMATION. 
Unauthorized disclosure and/or use of information contained in this
email 
is prohibited. If you are not the intended recipient, you may not read, 
use, disseminate or copy this message or any other files transmitted
with 
it. 



Victor Hernandez <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
07/08/2009 06:31 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
Re: [TN] Electroless Nickel Electroless Palladium Immersion Gold
(ENEPIG)






Dave,

   Can you share the reference material that you state in this note
concerning the above stated topic.   I want to be knowledgeable of the
process versus hard gold and pure ENIG for commercial use.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Thursday, April 23, 2009 10:41 PM
To: [log in to unmask]
Subject: Re: [TN] Electroless Nickel Electroless Palladium Immersion
Gold (ENEPIG)

Hi Lee - ENEPIG is a very good finish - look up the 1996 SMI conference 
proceedings where  Rockwell published a paper on the topic. One of the
big 
drawbacks of the finish is its cost. There are a couple of good
reference 
books that talk about ENEPIG. When I get back off business travel, I can

send your the exact references.

Dave Hillman
Rockwell Collins
[log in to unmask]




Lee Whiteman <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
04/23/2009 01:11 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
[TN] Electroless Nickel Electroless Palladium Immersion Gold (ENEPIG)






Does anyone have any opinions of using Electroless Nickel Electroless
Palladium Immersion Gold (ENEPIG) as a board finish for high reliability
aerospace applications?

You can contact me off line if necessary...

Thanks again.

Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2