TECHNET Archives

May 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Victor Hernandez <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 22 May 2012 08:09:43 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (39 lines)
Fellow TechNetters:

   I am very surprised that I have not had very many feedbacks on my initial hardness inquiry.   I would suspect that there would be many users of hardness testing out there.   Perhaps this time it will be a charm.   In a previous life I just used the instrument.   This time I want to understand the test and instrument.

Victor,

_____________________________________________
From: Hernandez, Victor G
Sent: Wednesday, May 02, 2012 7:47 AM
To: TechNet E-Mail Forum
Cc: Hernandez, Victor G
Subject: Hardness testing guidelines


Fellow TechNetters,

   What are some guidelines with regards to hardness testing,
Aluminum 384, ADC 12
Rockwell B, ball bearing, 1/16 inch dia. (0.0625 dia.)
Load:           100
Target:         53
Min coupon thickness:   ???????
Coupon Size:   ????????
Spacing between sites:   ???????
Coupon flatness:   ???????

My sample is:
Coupon thickness:       0.05425 inch
Coupon Size:            1.3 x 0.58 inch
Can the round indentation, diameter and depression, be used to confirm the instrument reading/value?

Victor,


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2