TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Date:
Wed, 3 Mar 2004 14:30:22 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Tremmel <[log in to unmask]>
Subject:
From:
David Tremmel <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (89 lines)
Hello,

Regarding your first example, chances are you have you have residual flux on
the boards although it depends on who, when and where they were
manufactured.
I have been doing repair of various types of PCBs for years and am confident
without seeing your examples that the residual flux between the leads of
your SMTs in nothing to worry about.

Your example of where the hand soldering was done is definitely an example
of flux residue.  When the heat of a soldering tool is applied to the flux,
the liquids evaporate and the heavier solids remain on the board and become
crystallized or become a very thick and tacky substance.

I am sure that the engineers in the TechNet forum could give you a more
technical answer, but I hope this helps in the meantime.

Have a nice day,

David

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bissonnette,
Jean-Francois
Sent: Wednesday, March 03, 2004 2:19 PM
To: [log in to unmask]
Subject: [TN] Flux Identification and Soldering over gold plated pads???

Got two questions here

First I would like to know if there is a way to identify flux residues on a
soldered assembly.  For instance, I have a series of
board that have a glass like residues between the lead (SMT) and quite a lot
of it.  It looks clear, little bit brownish and it
breaks like glass if I apply pressure with a dentist pick.  Also where hand
soldering was done, the brown color is much 
more obvious.

Second.  Any of you ever seen a board with gold plated lands  instead of tin
plated?  Well I would not be able to say it
it IS gold plated but it sure looks like it and not copper.  

Any help would be appreciated.

Jean-François Bissonnette
Vérificateur, Contrôle de la Qualité
Électronique
Produits et Procédés
Vapor Rail Inc.
10655 Henri-Bourassa O.
St-Laurent, Qc
H4S 1A1

(514) 335-4200 x2021
(514) 335-4231 fax



***** CONFIDENTIALITY NOTE *****
The content contained in this e-mail transmission is legally privileged and
confidential information intended only for the use of the individual or
entity named herein. If the reader of this transmission is not the intended
recipient, you are hereby notified that any dissemination, distribution, or
copying of this transmission is strictly prohibited.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2