"Elensky, Richard" <[log in to unmask]>
Date:
Wed, 5 Dec 2001 09:15:08 -0800
MIME-Version:
1.0
X-To:
Mark Charlton <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (60 lines)
Mark,

        We used a large stainless steel basket from EMC.  (20" x 20" x 2")
There are several others available.

        As the mesh was large (about .5" x .5") we lined it with stainless
screen.  The lining was not stretched tight, to provide some protection for
the small assemblies.

We were using a Hollis Hurricane aqueous cleaner with 10 hp wash/rinse
pumps.  Even with the small mesh screen we were able to adequately clean the
boards.

Hope that helps.

Rich


Richard Elensky
Sr. Manufacturing Engineer
[log in to unmask] <mailto:[log in to unmask]>

Tel:  559-292-1111  x246
Fax:  559-292-9355

Dantel
2991 North Argyle Ave.
Fresno, CA, 93727
Visit our web site at:
http:// www.dantel.com <http://www.dantel.com>


        ----------
        From:  Mark Charlton [SMTP:[log in to unmask]]
        Sent:  Wednesday, December 05, 2001 8:31 AM
        To:  [log in to unmask]
        Subject:  [TN] Small PCBs in wash

        We're experiencing some damage to some small PCB's (0.75"x1.75")
that occurs during their trip through the aqueous cleaner.  The boards are
originally processed in a panel but some require rework or additional
processing once they have been depanelized.

        Can anyone suggest a method to secure these small boards inside the
wash racks as to prevent this damage?

        Mark Charlton



---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2