In a message dated 9/4/2008 12:36:36 P.M. Eastern Daylight Time,
[log in to unmask] writes:
I've been dragged (kicking and screaming) out of my comfort zone, and am
looking at a wire harness. I've got some 0 awg wire to solder into a
connector. We haven't tried it, but I really doubt that my Metcal MX-500 system is up
to this task. Do any of you have experience with this, and if so can you
recommend equipment or technique?
-------------------------
I have had great success with the JBC heavy duty soldering station in such
situations.
Jon Moore
**************It's only a deal if it's where you want to go. Find your travel
deal here.
(http://information.travel.aol.com/deals?ncid=aoltrv00050000000047)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------