TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vjo5Q-0000TYC; Mon, 13 Jan 97 09:14 CST
From [log in to unmask] Mon Jan 13 15:
49:07 1997
Old-Return-Path:
Date:
Mon, 13 Jan 97 10:04:05 EST
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9154
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"zZk_z1.0.e7G.-4bso"@ipc>
Subject:
From:
X-Loop:
X-Priority:
3 (Normal)
Message-ID:
Parts/Attachments:
text/plain (24 lines)
Has anyone tried to achieve high levels of ionic cleanliness--e.g. 2 to 5 
micrograms per square inch of halides--on dry film solder mask using 
aqueous cleaning with or without saponifier added.  I would be interested 
in specific details of your successes or failures.  

Many seem to be able to achieve such levels with LPI.  If you have tried 
and failed do you have a generally accepted theory explaining why LPI can 
be cleaned more thoroughly without damage to the soldermask.

Thanks to S. Mikell for an enlightening reply to this question asked in a 
slightly different form.    

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2