TECHNET Archives

August 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Creswick, Steven" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 22 Aug 2001 10:37:22 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (65 lines)
Bill,

You should be able to get away with 30 microinches of gold.  I have gone
anywhere from 150-350 microinches of electroless, or electrolytic nickel
(subject to board layout constraints) with good success.

Word of caution - IMHO, if the board will sees multiple thermal excursions
(reflows - not to mention adhesive cure/s), and long WIP times (weeks)
before it gets to you, I would opt for heavy nickel, and going heavier on
the gold.  The reason for this is:  With each thermal excusion the base
copper tries to find pores/holes in the nickel to diffuse through/into.  If
successful, the gold is next.  Thermosonic gold bonding to corrupted gold is
problematic.  Thickness just delays the inevitable.  Nitrogen storage (at
least dry air) is assumed.

Steve Creswick - Gentex Corp



-----Original Message-----
From: Bill Christoffel [mailto:[log in to unmask]]
Sent: Wednesday, August 22, 2001 10:04 AM
To: [log in to unmask]
Subject: [TN] Ni/Au Plating Question


Ok all you plating guru's.......I am currently specifying a gold
(Thermosonic) wire bondable electrolytic gold for a new board design.
This in my mind was the easy part (Mil G-45204, Type III, Grade A, 40-50
microinches thick).    Now for the Nickel,   Currently we spec. a
Electrolytic Ni, 4-9% Phos., 150-200 microinches thick.

Questions:  Since my bonding is to the gold, is there a concern if the
Ni plating is Electroless or Electrolytic.  Which is easier to control ?
Which is a less expensive process ?  Any other concerns I should be
aware of ?

Thanks,
Bill C.

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2