Hello Dave,
is it possible to get a copy of these pages? What you describe seems to
be what we experience just now when we solder a ceramic filter on a
organic board with a heave brass backside. See attached files that you
can open in Adobe Photoshop.

I have also another delicate question for you as a TechNet guru: how on
earth do you He-test a large LTCC MCM with a soldered-on CuMo plate,
with soldered-on coax contacts outside the large sealframe, and also som
tantalum caps, also mounted on outside of the frame. All these outer
components together with the porous LTCC hides a lot of Helium and makes
the test a mess. The packages are laser seamwelded and He-bombed
afterwards. We have also tried to trim the He tester for a Nitrogene
peak instead, but with no useful result. Do you have any idea?

Finally, what is your e-mail adress for sending attachments directly to
you? [log in to unmask] does not work.Nor does 'dhillman...'

                                  Regards /Ingemar Hernefjord
                                   Ericsson Microwave Systems


> Hi Stephen - for additional info on grainy joints take a look at the
> following reference:
>
> "The Rough or Grainy Solder Phenomenon", R. Bulwith, PC Fab, October
1986,
> pages 23-35.
>
> In many cases a grainy solder joint is a cosmetic problem only. Good
Luck.
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2