Dear colleagues

We have some argues regarding PPM calculations, For an example: for
placement station of automatic SMT components, do we have to count the
soldering pads  or only the components.
If only the components its not the same level of difficult for capacitor
and fine pitch.
The same question is for dispensing machine of SMT glue.
Please E Mail me the general formula for PPM calculation.

Thanks and Best Regards

Rokah  Reuven

IPC Member

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2