TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Wenger, George M." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Wenger, George M.
Date:
Tue, 22 Jul 2008 10:31:31 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (99 lines)
Check out the IBM and Lucent NEPCON papers from the early 90's on Double

Reflow. 





Regards,

 

George

George M. Wenger

Andrew Wireless Solutions

Senior Principal FMA / Reliability Engineer

40 Technology Drive, Warren, NJ 07059

(908) 546-4531 (office) (732) 309-8964 (cell)

[log in to unmask]

 



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Dale Ritzen

Sent: Tuesday, July 22, 2008 8:44 AM

To: [log in to unmask]

Subject: [TN] They solder well... But they don't work!

Importance: High



Here's a good one for the collective "mind-meld"...



We have a two-sided, non-RoHS compliant, all-SMT assembly (no PTH parts)

that is reflowed under a leaded profile (cooler reflow temperatures than

Pb-free). There is one 44-pin QFP on the topside of the board that

consistently solders well (i.e. passes all IPC-A-610 Class 2 inspection

criteria), but fails test until it is reflowed with a hand iron, a

little flux and wire solder. We have about a 25% pass rate without

reflowing the QFP. That jumps to around 95% once the QFP is reflowed.

Several different date codes of the device have been tried with similar

results.



Thinking the ENIG pads under the device leads might be contaminated, we

cleaned them on several test case 4-up panels, with no change in yield.

Thinking it might be contaminated leads on the devices, our process guys

gently scraped off the tinned coating on the leads of several devices

and took it down to the Beryllium Copper finish. Same resultant yield.



We've re-run the failing assemblies through a higher reflow temperature

with extra "tacky flux" on them, trying to get a better reflow and use

the action of the flux to purge any contamination that might be

interfering in the solder junction. When done, the solder junctions on

the device look like a "Target - Class 1,2,3" picture from IPC-A-610,

but the yield is still around 25% unless we reflow the junctions with an

iron, some flux and wire solder.



There may be some things we're overlooking, but it's coming down to

where we believe the wire bonds to the lead frame material could be the

source of the problem. The intense, direct heat of the soldering iron

might be enough to generate a reflow of the wire bond, resolving any

bonding issues. But, on several different date codes? I will be getting

the vendor involved shortly to test the devices and see if they come up

with something. I'm fairly skeptical about doing this as typically the

normal answer I get is "all is working as designed".



We are all scratching our heads on this one... Any "words from the wise"

would be appreciated!



Thanks!

Dale Ritzen, CQA

Quality Manager/ISO Management Representative Austin Manufacturing

Services

Email: [log in to unmask]



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0 To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------



------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------------------------------

[mf2]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2