At 04:03 PM 11/26/96 -0800, you wrote:
>Hello Technetters!
>
>We have some boards where we have to use a no-clean flux in the
>THT process. Today we are haveing problem with thease boards 
>in the In Circuits Test where we don't have any neadle acces beacuse 
>of the flux resiudals after wave soldering.
>Today we are using Hollis PT500 with Hollis ultra spray station and
>Lonco 23F flux.
>We are now looking at some new flux and I want to here if some of 
>you have hade the same problem and how you solved it.

-------------------- Reply --------------------------------------------

Hi, 

Try Interflux IF2000.. It might help.

+====================================+
Kong Hui  Poh
Process/Equipment Engineering Advisor..
Techgate Electronics
Email: [log in to unmask]
=-=-=-=-=-= -=-=-=-.=.=.=.=.=.=.=.=.=.=.=.=. =.=.=.


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2