TECHNET Archives

November 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="ISO-8859-1"
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Wed, 27 Nov 2002 08:29:00 +0000
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Mark Austin <[log in to unmask]>
Subject:
From:
Mark Austin <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (55 lines)
As a Panasonic user myself, I have never come across this problem. There are
(usually) some additional Vision Codes that can be used for parts with dull
terminations. Ask the Engineer to refer to the Vision Code Manual and check
the Part Code and Part Type settings.

Mark Austin
Production/Process Engineer

ACW Technology Ltd.
(UK)

===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
26/11/02 16:57
>Thanks for your interest.
>The machine is a Panasonic MSR system.
>The SMT group would not like to change/adjust the vision system because it
>is/was working fine for all other reels.
>My argument is that perhaps the vision window is too small.
>They are contenting that the component is defective because the tin coating
>is dull.
>I would like to gather as much info as possible on component specification
>before I approach the component manufacturer.
>
>
>
>Francis Sun
>MARK IV Industries
>(905) 624-3025 ext. 1235
>Fax: (905) 624-4572
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2