TECHNET Archives

March 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
Date:
Fri, 8 Mar 2002 12:31:12 +0800
MIME-Version:
1.0
X-To:
Ken Patel <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (95 lines)
Hi, Ken,

I believe ENIG (or any other plating) can be applied either before or after
soldermask, but normally it's applied before to save on plating solution
costs among other things.

Yes, the immersion gold process is aggressive, so be sure your fab house is
using an ENIG-compatible mask. This often involves using an alternative
hardener in the mask mix, and it's better if your pads are not solder mask
defined, as the plating tends to get underneath the edges.

Masking from one side only, the holes can be cleaned, but it depends to a
large extent on the diameter of the holes and the capability of your fab
house. 10  mils and above, I believe, are OK, but smaller than that, the
cleaning process may have trouble penetrating properly and cleaning out the
bottom of the holes. I suggest you leave the holes open at both ends unless
you absolutely have to mask one end.

Peter




                    Ken Patel
                    <[log in to unmask]        To:     [log in to unmask]
                    OM>                  cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST
                    Sent by:             Aero/ST Group)
                    TechNet              Subject:     [TN] Fab Process question related to
                    <[log in to unmask]        ENIG
                    ORG>


                    03/08/02
                    01:40 AM
                    Please
                    respond to
                    "TechNet
                    E-Mail
                    Forum.";
                    Please
                    respond to
                    Ken Patel






At what stage the electroless nickel and immersion gold process is
applied, is it after the solder mask application or before? I believe
normally it is after the solder mask application but I want to verify
it. I have heard that chemistry involved is very nasty if left on the
board. If I plug or mask via holes from one side, I want to make sure
that there is no residue left of that nasty chemistry. Can it be cleaned
if mask from one end? Any comments?

re,
Ken Patel

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------





[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2