Trivia -- This is one of the ways that police departments bring up
fingerprints by using fumes from the glue to make the finger prints appear.
At 02:22 PM 6/1/99 -0400, you wrote:
>Hello,
>
>Here's a good one!
>
>The boards one of our touch-up ladies is doing ECOs on started making
>fingerprints appear after applying the wire bonding glue.
>That is, once the small glue dots are cured, all around them and in the
>adjoining areas, a white stuff, like baby powder, is appearing, making wide
>bands where the fingerprints show.
>
>Did anyone else experienced this? I assume it's a reaction between the
>perspiration and the glue. Is there any way to fix it, except gloves?
>
>The glue is Loctite 382. Is it the only troublemaking glue?
>
>Thanks, Ioan
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
--
------------------------------------------------------------
David E. Robertson (908) 245-6200
Sales Manager (908) 245-6176 fax
Hexacon Electric Co.
161 W. Clay Ave.
Roselle Park NJ 07204-1946
e-Mail: [log in to unmask]
URL: http://www.hexaconelectric.com
------------------------------------------------------------
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|