The best thing to do is to get a better price from your recyler on solder paste since by weight it is all virgin solder.
It should not be be priced as solder dross by weight for the obvious reason.
If you had the EVS solder recovery system then you could have the flux burned off in that system and return all that virgin solder to the wave, in ingots. These systems are offered with various filter systems and both can be portable so select an area that best suits your factory.
John Goulet
Process Engineer
----- Original Message -----
From: "Graham Collins" <[log in to unmask]>
To: [log in to unmask]
Sent: Thursday, April 2, 2009 2:59:57 PM GMT -05:00 US/Canada Eastern
Subject: Re: [TN] Solder Paste In the Solder Pot
Hi Kenny
I tried that - once! Biggest issue for us was the huge cloud of fumes
from the flux burning off - totally swamped the venting system on the
wave machine.
regards,
- Graham
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Thursday, April 02, 2009 3:43 PM
To: [log in to unmask]
Subject: [TN] Solder Paste In the Solder Pot
I have what I hope is a generic question without getting into too many
details.
IF the flux in the solder paste and the flux in the wave solder are
compatible and they are both 63/37, can unused, expired shelf life,
solder paste be dumped into the wave solder pot?
Thanks,
KennyB
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|