TECHNET Archives

March 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Dave Schaefer <[log in to unmask]>
Date:
Wed, 14 Mar 2018 13:21:29 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Yuan-chia Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Yuan-chia Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"; delsp=yes; format=flowed
MIME-Version:
1.0 (Apple Message framework v753.1)
Parts/Attachments:
text/plain (12 lines)
SAC is relatively strong under compression, but underlying Cu cct  
might not be under pressure (consider each Ball as  point contact).  
you might need to do FEM to find out.. for example, if you have via  
in pad, you might damage the via before compressed SAC ball (same  
apply for the BT-substrate on component side).  IMHO.
On Mar 14, 2018, at 12:49 PM, Dave Schaefer wrote:

> Does anyone have any references to good information regarding the  
> amount of compression that can be applied to an SAC BGA component  
> for heat sinking purposes? We want to maximize our thermal  
> performance without sacrificing solder joint & component reliability.