TECHNET Archives

May 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Ken Bloomquist <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Bloomquist <[log in to unmask]>
Date:
Tue, 4 May 2010 12:54:16 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (53 lines)
Inge,

By your statement (maybe their statement) "... few solder joint reliability
problems when mixing SnPb and LF components and solder alloys."

Doesn't that imply that that they are mixing lead into the solder joint in
one way or another, "mixing SnPb and LF". I would think that any amount of
lead added would help.

KennyB

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Tuesday, May 04, 2010 1:36 PM
To: [log in to unmask]
Subject: Re: [TN] Why not Pb-free?

You reminded me of a report from NPL-2005.  In cooperation with Aeroflex, 
Alcatel, BAE, Bosch, Goodrich, RR, TRW and some more.  A very advanced 
investigation with lots of solders with Pb and without Pb. The titel was: 
Measuring the Reliability of Electronics Assemblies during the Transation 
Period to Lead free Soldering.  The foreword had this content:
"The work has indicated that there should be few solder joint reliability 
problems  when mixing SnPb and LF components and solder alloys. Very few 
thermal cycling fatigue failures were experienced. Not one single failure 
was generated during the harsh vibration  testing ".

I can't scan all these pages, however, if someone, not to many, are 
interested, I can send it offline.  You can probably get it from NPL 
directly yourself.

Very optimistic result at that time.   Just wonder how they feel today. 
Anyone from NPL?

Inge



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2