Hi Inge!
I am also someone who takes stuff to pieces. You should see the scars on my knuckles from all of the sheet metal cuts you can get on a car.
Now that you've put your car back together....
Are you absolutely sure the solder joint was bad when it left the line? I mean, the rest of the joints look just fine, so what is it about that one? In all liklihood this was wave soldered.
What if the real problem is that too much current is going through that joint, which is considerably smaller than the adjacent joint on the same trace? You may have only peeled back the first layer of the onion!
I hate to put doubts in the mind of someone who did an excellent job getting the thing repaired, but I know you are tough!
Wayne
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Tuesday, July 14, 2009 3:55 AM
To: [log in to unmask]
Subject: Re: [TN] NTC (It's not Friday, but this is so true!)
Inge - wow! It's all in the hunt! Good find!
Steve - You are right! That is a cool trailer!
Steve C
http://stevezeva.homestead.com/files/Inge_s_Car_Fun_.pdf
http://stevezeva.homestead.com/files/Unusual_Trike.jpg
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|