Michael,
The main problem I saw when we used (25 yrs ago) PWBs that were rolled was
solderability. Shelf life was short. I remember this method as being able
to cover dirty copper and you wouldn't know you had wetting problems until
you tried to solder the assembly.
Gary
----- Original Message -----
From: "Michael Bell" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, March 24, 2003 2:39 PM
Subject: [TN] Roller Tinned PCB's
> Hi all,
>
> Just a little stumped on terminology here, what is "Roller Tinning". What
> is the specific differences between this method and HASL??? Are there any
> specific pros/cons for the Roller method??? Any information would be
> appreciated.
>
> Cheers
>
> Mike
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|