TECHNET Archives

September 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 14 Sep 2011 09:20:05 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Cedric ORAIN <[log in to unmask]>
Message-ID:
<03c501cc72ae$bb5ad570$32108050$@[log in to unmask]>
Subject:
From:
Cedric ORAIN <[log in to unmask]>
X-cc:
Emmanuel DURET <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (54 lines)
Good morning again !

 

This is the second subject for which I need your help today. During previous
work -when I qualified lead free assembly years ago- several PCB finitions
was compared. Among the finitions we tested, HAL Sn100C was rejected because
of reflow issues using SAC305 solder paste. 

 

Problems were lack of solderability. I assumed that the reason was because
of the difference between liquidus of Sn100c in comparaison with SAC305. We
didn't make a lot of work to solve that as we head quickly to ENIG and I
finally rejected Sn100C. until this week when a customer request Sn100C for
cost reason.

 

So I would appreciate testimony of technetters that use successfully Sn100C
as PCB finition with SMD process as well as troubleshooting feedback
regarding this process.

 

Regards,

 

Cedric

 <http://www.inovelec-group.com> www.inovelec-group.com

 

 



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2