TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vnWkY-0000bOC; Thu, 23 Jan 97 15:31 CST
Content-Type:
text/plain; charset=us-ascii
Old-Return-Path:
Date:
Tue, 23 Jan 1996 23:43:25 +0000
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9560
TO:
Return-Path:
<TechNet-request>
X-Status:
X-Loop:
Resent-Message-ID:
<"E1C6c.0.mc.CZzvo"@ipc>
Subject:
From:
gabriela <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Message-ID:
X-Mailer:
Mozilla 3.01 (Win16; I)
From [log in to unmask] Thu Jan 23 16:
47:37 1997
Parts/Attachments:
text/plain (27 lines)
Hello,technetters!
We perform double reflow on boards populated with SM LEDs on one side
and on the other side SMCs and PTH connectors.
In order to prevent the LEDs to go twice through hgh temperature
profiles -the second one being even loger-we tried to use a solder
paste with a lower melting point:Sn43Pb43Bi14 which is not eutectic.
The cross section of the pin in hole showed some solder voids-which
were present also when using Sn63 paste and are accptable from our point 
of view-but also cracks which originated from them along the pin or
along the hole wall.Our boards are 0,1microns gold plated.
Could anyone explain why it happed and give us some advice?

Gaby
P.S.Thanks to CONDOR and DAVE HILLMAN for their former replies!

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2