If you are using turkey bags, the longer you can hold under vacuum before
pressing, the better.  Turkey bags tend to seal tightly around the lamination
book, making it difficult to evacuate all the moisture within the package.  I
typically recommend 45 minutes for turkey bags, out of the press, if you can.

Vacuum assist presses, on the other hand, are much more effective than turkey
bags.  The press chamber seals tightly, but leaves open areas around the
lamination book.  This allows moisture to boil out of the package quickly.
 Typically, 10 to 15 minutes hold in a vacuum press is sufficient.

Mark Dowding
Regional Technical Specialist
Insulectro

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2