Thanks Steve,
A follow up question: Does the copper then get more brittle? To a point that
the processing should change?
Joe
Quoting Steve Owen <[log in to unmask]>:
> Joseph,
>
> Anneal
> 1 To temper or toughen (something) by heat treatment to remove internal
> stress, crystal defects, and dislocations.
>
> Steve.
>
> -----Original Message-----
> From: Joseph Spicuzza [mailto:[log in to unmask]]
> Sent: 10 January 2002 15:48
> To: [log in to unmask]
> Subject: Re: [TN] hole wall pull away and resin recession
>
>
> Rich,
> I must be braindead this morning, expound on "anneals" if you would,
> rather, remind me what that means.
> Thanx
> braindead Joe
>
> Quoting [log in to unmask]:
>
> > Joe
> >
> > remember that baking also anneals the copper
> >
> > Rich Fudalewski
> >
>
>
>
> Joseph Spicuzza
> Quality Assurance Supervisor
> Advanced Interconnect Products Division
> Compunetics, Inc.
> ph: 412 858-6166
> fax 412 373-8060
> [log in to unmask]
>
> ----------------------------------------------------------------------------
> -----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
> SET
> Technet NOMAIL
> To recieve ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases
> >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700
> ext.5315
> ----------------------------------------------------------------------------
> -----
>
> This e-mail has been scanned for all viruses by Star Internet. The
> service
> is powered by MessageLabs. For more information on a proactive
> antivirus
> service working around the clock, around the globe, visit:
> www.star.net.uk
>
> ------------------------------------------------------------------------------
---
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
> SET Technet NOMAIL
> To recieve ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases
> > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> ------------------------------------------------------------------------------
---
>
Joseph Spicuzza
Quality Assurance Supervisor
Advanced Interconnect Products Division
Compunetics, Inc.
ph: 412 858-6166
fax 412 373-8060
[log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|