Bare boards may have some hidden defects which would affect their reliability but won't manifest themselves right away. What I'm getting at is that cross-sectioning through specific areas has to be done fore qualification of a PWB
Vladimir
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
-----Original Message-----
From: John Balchunas <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Wed, 9 Nov 2011 14:23:39
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
John Balchunas
<[log in to unmask]>
Subject: [TN] Qualification of PWB Suppliers...
All,
Does Final Assembly and Functional Testing add value to Qualifying Bare
Board PWB Suppliers?
Put another way...is a Supplier's Continuity/Isolation/Controlled Z
Testing, and their Customer's Inspection of the Physical Product to its
Documentation, sufficient to Qualify the Supplier without additional
Assembly or Functional Testing?
Thanks in advance for sharing your experiences with this.
John Balchunas
Supplier Quality Engineer
Email: [log in to unmask] <mailto:[log in to unmask]>
Tel: 763-278-2249
Fax: 763-767-4635
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|