Carlone,
MIL-P-13949 went obsolete as of Nov. 30 1998. The replacement is IPC-4101.
Also GFN is FR4.
> Approved-By: [log in to unmask]
> MIME-Version: 1.0
> Date: Wed, 24 Feb 1999 12:31:25 -0500
> From: Carlone Anthony C NPRI <[log in to unmask]>
> Subject: [TN] FR4 PWB Material
> To: [log in to unmask]
>
> Hello there, IPC/IPC Members!
>
> I work for the Naval Undersea Warfare Center (NUWC) in Newport, RI. My job
> function involves the manufacture and acquisition of MK 48 ADCAP Torpedoes.
>
>
> We're having failure problems with PWB's whose master dwgs specify core
> material and prepreg material per MIL-P-13949, slash sheets 4 and 12.
> Specifically, the dwgs require core material of GFN and prepreg material of
> PGFN. However, the PWB supplier made the boards of "FR4" material.
>
> So, with that background, would somebody out there in the IPC world please
> answer a couple of questions for us:
>
> 1. What is FR4, and what is the parent spec that addresses or controls it?
>
> 2. Are there any commercial (IPC or somebody else's) and/or military
> performance specs that directly correlate with or directly substitute for
> MIL-P-13949 slash sheets 4 and 12?
>
> Any help or guidance you can give us would be greatly appreciated!
>
> Thanks!!
>
> Tony Carlone
> e-mail: [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
>
Regards,
Jerry Schwartz, CID
IPC Certified Interconnect Designer
"May the Schwartz be with you"
###################################################
# Jerry Schwartz,CID Designer 3 #
# Harris Corporation GCSD Voice (407)-727-5474 #
# P.O. Box 91000, MS 1/5852 Fax (407)-729-7540 #
# Melbourne, FL 32902-9100 Pager (407)-690-9797 #
# mailto:[log in to unmask] #
# http://harris.com #
###################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|