> I have a board which has failed shock and vibe testing, due to a SMT
> component breaking off. I have been told to use an RTV to hold the part
> on.
> Could I please get some help. What is an RTV? Who do I get them from? Is
> there automated ways of applying? I would be more than happy to hear from
> vendors, but maybe they should respond directly to me.
> Thanks.
>
> Steve Quinn
>
Steve,
RTV is a silcon sealant - like the stuff you put round the edge of your bath to
stop it leaking. RTV is Dow Corning's trade name for it's family of sealants.
If you really want to use this to stop the device leaving the board, make sure
you get hold of a grade that doesn't liberate acetic acid on cure. Normally
it'll tell you on the side of the tube and if it does it'll smell of vinegar.
You can probably tell that I wouldn't rate this as a solution to your problem -
but good luck anyway!
Eric Christison
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|