TECHNET Archives

September 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Seth Goodman <[log in to unmask]>
Reply To:
Seth Goodman <[log in to unmask]>
Date:
Thu, 2 Sep 1999 15:30:01 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (89 lines)
Sean,

I agree with John's answer.  Note that aluminum is a poor contact material
due to the formation of very hard oxides that have very high dielectric
strength.  In addition to the oxide inhibiting paste John refers to, you
might want to try a different surface treatment for the aluminum, such as
iriditing.  I use this routinely on aluminum chassis parts that have to mate
with RF gaskets.  I don't know about its long term resistance to oxide
formation, however.  Anyone care to comment?

Seth Goodman
Goodman Associates
7687 Leta Way
Verona, WI 53593-8631
Tel (608)833-9933
Fax (608)833-9966

> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Sean Hager
> Sent: August 30, 1999 4:24 PM
> To: [log in to unmask]
> Subject: [TN] Electro-mechanical connections for Power Applications
>
>
> Hi Group!
>
> I am currently having troubles with a terminal connections to the +5V
> output of a switching PS.  The current configuration basically consists of
> 0.5"x0.7"x0.060" aluminium bus bar (with hole for hardware),
> connected to 2
> 8guage stranded cables, via 2 8guage red ring lugs (tin/lead plated
> copper).  These are connected using 8-32 Screw and Hex nut w/ lock washer.
> This is my list of questions:
>
> Is the standard torque for this hardware type adequate for 50+ amp
> capacity?
>
> Do the ring lugs or bus bars require any preparation (cleaning, scoring,
> etc.) prior to assembly?
>
> Are there any special concerns with the dissimilar metals?
>
> How would you (or what standard would you use) to join this harness and
> terminal?
>
> I have seen a full 200mv across the bus bar/ring lug junction at [log in to unmask]
> There is no visible corrosion on either termination, and the hardware
> torque was approx. 15-20 kg-cm.  Generally this connection has been very
> reliable for about 5 years, lately we have seen a notable rate of low
> output on 5V attributed to "contact resistance" while loaded.  The
> manufacturer (Power Supply) has no hardware or installation guidelines.  I
> could best describe this as the "loose battery terminal effect"
> as compared
> to an automobile.  Is the solution realy as simple as clean and tighten?
>
> Thanks,
> Sean
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2