3M offers some ESD tapes (low charge generating, need to use their
conductive dispenser) that are either acrylic(?) or rubber adhesive based -
they can leave residue after thermal curing even though they are billed as
low to no residue.
Mike
Rob Carrillo
<[log in to unmask] To: [log in to unmask]
OM> cc:
Sent by: TechNet Subject: [TN] Conformal Coat ESD Tape
<[log in to unmask]>
02/11/2005 10:33
AM
Please respond to
TechNet E-Mail
Forum; Please
respond to Rob
Carrillo
Is anyone aware of a Conformal Coat ESD Tape that might be available? We
currently use what is essentially painters tape because is does not
leave adhesive residue.
I noticed a post in the archives regarding ionizers at the workstation
which may be an option.
Thanks,
Rob Carrillo
Quality Manger
North Atlantic Industries
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc. It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|