Hans,
I'm not sure if this will fit your bill, but when I was in the military
doing electronic repair I found out that those spray contact cleaners for
electronic components works real good after spaying it into a clean soft rag
for adhesive gum (residue) removal. I'm not sure of the cost constraints
but I'm sure it can also be purchased in gallon cans also. We were using
some made by a company called LPS but I can't find a website on them. If
you're located near a military base you might want to try making contact
with any electronic repair shop and ask for assistance. I've found out that
the Radio Shack/Tandy stuff is not good.
Email me direct if you have any other questions.
Thanks,
-Gary
-----Original Message-----
From: Hinners Hans Civ WRALC/LYPME [mailto:[log in to unmask]]
Sent: Thursday, July 13, 2000 4:41 PM
To: [log in to unmask]
Subject: [TN] Adhesive Remover for artwork
Hey Gang,
I'm looking for an adhesive remover.
We're using a new label printer to image the batch numbers on the panels.
Only problem, the labels are leaving adhesive on the artwork when we pull
them off. I already tried Chemtronics adhesive remover and it just smeared
the glue around. So, before I start making a bunch of calls or trying
household cleaners I thought I'd ask this illustrious body.
Thanks,
Hans
~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Materials (Process & Manufacturing) Engineer
Warner Robins Air Logistics Center
Avionics Production Division
Manufacturing Branch
380 Second Street, Suite 104
Building: 640, Mail Stop: LYPME
Robins AFB, GA 31098-1638
Voice: (912) 926 - 1970 Fax: (912) 926 - 7164
mailto:[log in to unmask]
http://www.robins.af.mil
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|