TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Terry L. Munson" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 29 May 2009 16:11:22 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (63 lines)
Lenny 
I would suggest a different non-chemical approach by freezing the ballast  
and then chipping or cutting the frozen pitch material to get to the surface 
for  Failure Analysis.  We have found that pitch can be contaminated and 
cause  leakage and corrosion problems. We have also found that capacitors can 
leak and  the electrolyte will dissolve the material and cause leakage and 
corrosion  problems.  If you have solder joint problems then this approach 
works well  to investigate the joint quality as well.  If you have an question 
please  call.  
Terry Munson
765-457-8095
 
 
In a message dated 5/29/2009 2:01:42 P.M. Eastern Daylight Time,  
[log in to unmask] writes:

We have  a lighting ballast in for failure analysis and arent sure how to 
get the  encapsulant "tar" from it?
This is a lighting ballast and we have the metal  covers removed and are 
left with a ballast assy built on a pcb, and covered in  a thick,  black,  
semi-pliable, tar-like encapsulant. 
The  tar-like encapsualant smells just like roofing tar.  If you lay it on 
a  piece of notepaper it stains it just like roofing tar.  It can be peeled  
away just like a roofing tar.  We are afraid of poking too much and  
damaging components or circuits.  Anybody have experience with it? - and  know 
what it is?  and how to let it soak in a pan of something and rinse  this stuff 
of instead?  Better ideas?
Thanks in advance,
Lenny  Carter
Design Engineer
ERG, Inc.
ph (607) 754-9187  x3063
www.ergpower.com

---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To  receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]:  SET Technet Digest
Search the archives of previous posts at:  http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information,  or contact Keach Sasamori at [log in to unmask] or 
847-615-7100  ext.2815
-----------------------------------------------------

**************We found the real ‘Hotel California’ and the ‘Seinfeld’ 
diner. What will you find? Explore WhereItsAt.com. 
(http://www.whereitsat.com/#/music/all-spots/355/47.796964/-66.374711/2/Youve-Found-Where-Its-At?ncid=eml
cntnew00000007)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2