TECHNET Archives

March 2018

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Wayne Showers <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Showers <[log in to unmask]>
Date:
Wed, 28 Mar 2018 14:34:03 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (10 lines)
To contrast slightly with Dave, 3 reworks was established by procedure and was a direct result of preparing for NADCAP certification.
For BGA's, we established a 1 and done guideline for rework so that the assembly was evaluated if a second rework was to be attempted.  This was done mostly as a function of the component cost, but also to minimize potential pad damage.

Rework limits are mostly driven by the diminishing bond strength of the functional epoxy.

Here are the general guidelines:
Note, Prepreg is chemically almost identical to DEVCON 2-ton epoxy.  This has a bond force of 15.5N / mm2, but each successive heat cycle weakens the bond by hardening (crystallizing) the epoxy.

Hardening (crystallization) at temperatures above 300C, decomposition at temperatures above 350C.  For my non-metrically inclined, 572F and 662F.