Hi all,
We recently had a problem on a assembled part that had some kind of liquid
residues between lands
on the pcb. It is conductive and would not evaporate even if heated up with
a heat gun. In some
other areas the residues (don't know if they are of the same origin) had
more the apprearance of syrup.
Anyone can tell me what this is?
Thanks in advance!
Jean-François Bissonnette
Vérificateur, Contrôle de la Qualité
Électronique
Produits et Procédés
Vapor Rail Inc.
10655 Henri-Bourassa O.
St-Laurent, Qc
H4S 1A1
(514) 335-4200 x2021
(514) 335-4231 fax
WABTEC CORPORATION CONFIDENTIALITY NOTE
The content contained in this e-mail transmission is legally privileged and confidential information intended only for the use of the individual or entity named herein. If the reader of this transmission is not the intended recipient, you are hereby notified that any dissemination, distribution, or copying of this transmission is strictly prohibited.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|