Hello Technetters,
We experienced some problems after reworking circuit boards, I would like to have inputs on the following.
The problem found is capacitor leakage. The capacitor was added manually after automated production. The boards were coated with acrylic conformal coating.
1- How should a WS flux be cleaned after a rework?
2- Can WS be cleaned with alcohol? If not what would happen?
3- When reworking a SMT component, can WS flux be trapped under the component and cause leakage. The rework was cleaned with a brush or similar method.
We think that the rework method was as follow (to fix a possible contamination under the component)
a- SMT component is removed (possibly directly through the conformal coating)
b- Using coating thinner, the area is cleaned and verified under UV to ensure no coating is present.
c- WS flux is added
d- Component is soldered back in place
e- Area is cleaned with isopropyl alcohol
f- Coating is added
I think I've read that cleaning WS flux with alcohol is a NO NO! Can anyone confirm and comment?
Jean-Francois
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|