How much of EMF change after aluminum is anodized (chromated) depends on 
how good/thick the coating is.  It is fairly easy to measure the relative 
potential delta of two materials.  Check the book "Corrosion Engineering" 
by Fontana/Greene or any other electrochemistry book and you'll know how to 
do it.  Remember, (1) surface area is an important factor, (2) Redox 
(reduction/oxidation) potential is only a thermodynamic indicator, i.e., 
the tendency to corrode.  It does not provide kinetic information, i.e., 
how fast it corrodes.  

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2