TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Franklin D Asbell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Date:
Mon, 25 Sep 2006 18:03:59 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (77 lines)
6 of one, 1/2 dozen of the other.

You should consider many factors in regards to which is preferable, for
example, shelf-life, handling, packaging, number of thermal cycles the
product will see, surface features, size/pitch, etc.

In my opinion, handling durability is better with immersion tin; shelf life
is better with immersion tin, and solderability are equal when measuring the
same feature types.

This is comparing the Omikron with the Macdermid Sterling Silver, and, most
important, both baths operating optimal.

The Omikron bath is more difficult to maintain than the MacDermid SS but if
I had to choose one over the other it would still be the Omikron. The
thickness of the Omikron needs to be on the high side (30 - 40 micro") in
order to pass multiple thermal cycles, I've not seen silver pass as many
with similar results as tin.

Again, there are many factors you should consider, keep asking questions,
talk to suppliers, customers, run DOE's, get your hands dirty and you will
find what suits you best, this is just my opinion.

Franklin

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of kwood716
Sent: Monday, September 25, 2006 4:25 PM
To: [log in to unmask]
Subject: [TN] PCB Finish

Hey all,
Question...
Is immersion silver a more reliable and all around better finish than white
tin? I am looking into using it instead of the Omikron OA-8 we currently use
and would like some input.
Note: I can't use and nickel in the PCB, these boards are for MRI use and
have to be completely non-magnetic.
Thank you
Ken

  _____


Saturn PCB Design, Inc.
Kenneth J. Wood CID
2737 Bishop Lane
Deltona, Fl 32725
Phone: 407-340-2668
email:  <mailto:[log in to unmask]> [log in to unmask] www.saturnpcb.com
<http://www.saturnpcb.com/>



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2