TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Werner Engelmaier <[log in to unmask]>
Date:
Sat, 3 Jul 2010 12:48:47 -0400
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (224 lines)
Hi,

 I operated a wave machine for several years, when a PCB comes off it is
very hot and very soft. Flexing while in this state could cause problems.

Bob Kondner

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Friday, July 02, 2010 9:30 PM
To: [log in to unmask]
Subject: Re: [TN] Cracked 2208 smt resistor end joint

 Hi Eldon,
I am surprised you ave not seen failures like these earlier.

 Also, did you perhaps switch to Pb-free solders?




My present theory is the crack occurs when the assembly is wave soldered
causing excessive tension on the resistor due to CTE mis-match, and some of
these crack.



Sorry, but this is wrong. On heating the PCB expands more than the CC-no
cracking.


But when the board comes back to ambient it seems to be
longer, and shows a gap.

On cooling, the PCB shrinks more, putting the CC, solder joints and all in
tension-causes cracking and gaps.


After a board goes through 3 heat cycles at a CM,
wouldn't it be stable in CTE?

No, there is no 'stabilization' of CTE's.


And why would the other resistor not have the
same issue?  Is CTE different in X and Y?

There are differences in CTE in x and y-by sometimes more than 2 ppm/C. The
loading is also different if running parallel or perpendicular to the wave

Finally, would an error or change in
the raw fab process cause a change in the CTE and cause this issue to occur
after many years?


Obviously, something has changed-you need to find out what.

Werner









-----Original Message-----
From: Eldon Sanders <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, Jul 2, 2010 7:31 pm
Subject: [TN] Cracked 2208 smt resistor end joint


We are experiencing fractures in the end metallization or solder joint on
one of



two larger high voltage resistors, size 2208.  They are mounted on FR-4.

Only one location is failing.  The other location is an inch away and
oriented

at

90 degrees.  The failure rate is variable between assembly lots.  Some have

no failures, and no observed cracks.  The most recent lot has a 2% failure

rate, and another 2% that exhibit visible cracks in the ceramic but the
solder

joint is connecting the pad to the metallization and making electrical

connection.  I believe the root cause is the poor choice of the FR-4 board

material with such a large ceramic resistor.  However, about 80,000 boards

have been built over 7 years without this failure mode.  So, I am searching
for

the root cause of this specific timeframe.  I have verified the process at
the

CM has not changed - the resistor is mounted on the 2nd pass SMT, and the

board goes through wave soldering of TH components using a fixture.  The

same date code resistor is used for both good assembly lots and bad.  There

is some correlation to the date code of the bare fab.  On cracked boards

there is a gap observable between the solder joint and the ceramic resistor

body.



My present theory is the crack occurs when the assembly is wave soldered

causing excessive tension on the resistor due to CTE mis-match, and some of

these crack.  But when the board comes back to ambient it seems to be

longer, and shows a gap.  After a board goes through 3 heat cycles at a CM,

wouldn't it be stable in CTE?  And why would the other resistor not have the


same issue?  Is CTE different in X and Y?  Finally, would an error or change
in

the raw fab process cause a change in the CTE and cause this issue to occur

after many years?



Thanks to all the incredible minds if TechNet.



Eldon Sanders

Sr. Manufacturing Engineer

Welch Allyn Monitoring

8500 SW Creekside Place

Beaverton, OR 97008-7107

phone: (503) 530-7596         fax: (503) 526-4300

[log in to unmask]



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2