Hello,
I am getting ready to qualify a new cleaning process using IPC B-36 test
coupons and I am looking for suitable components for the test. The board
was designed for the use of a 68 pin LCC or PLCC. The footprint is
about .800 mils inside pad to pad square. The pad length is apx .100 mils.
The problem with the components mentioned above are:
The PLCC from Practical Components has a standoff height of about .020 mils
and the LCC fits tight to the board with no stand off at all. If I use the
LCC I will likely fail the SIR testing because I don't think I can get
under it to clean completely. If I use the PLCC, I will clean it ok, but I
don't feel that it is a practical representation of what we see in
production. I would really like to find a QFP that would fit this footprint
and that I can form to a more realistic standoff height. Does anyone have
any suggestions?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2