TECHNET Archives

February 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Becerra Alejandro <[log in to unmask]>
Date:
Fri, 23 Feb 2001 18:08:54 -0500
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Becerra Alejandro <[log in to unmask]>
Parts/Attachments:
text/plain (30 lines)
Hello To All,

Thanks for your help in rework temperatures.
Now I have a question regarding to torque value in 0603 components attached
with adhesives.
We use adhesive to attach SMD components in the bottom side of the boards
before the wave solder process.
We use torque test to evaluate the adhesion of the glue to the board and
component.
We are introducing 0603 components and we are interested in the appropriate
torque for these components.
The data that we have for 1206 components is 3.5 N-cm.

Thanks

Alejandro Becerra
Quality Assurance
Phone (915) 841-8439, Fax (915) 841-8401
[log in to unmask]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2