Agreed the benefits of Pb free solders are at best moot, but ....
so far as 113 Freon is concerned objective measurements showed it was not
actually much good as a cleaner. In fact for most people it was like giving
up cigarettes, once you managed to shake the habit you were actually better
and richer.
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of - Bogert
Sent: 01 May 2006 22:43
To: [log in to unmask]
Subject: Re: [TN] NTC Thank you for all of your support for Pushback
May 1, 2006
In my opinion its time we treated RoHS just like drugs. That is, "just say
no" to lead-free in electronic solders. If enough industry folks say no,
lead-free may hopefully die. Folks across the "pond" have created an
environmental monster with little tangible saving of our environment, with
much technical risk in eliminating lead from solder. Its kind of like ISO
9000, a vehicle for a lot of folks to make a lot of $.
Look what took place when folks banned Freon as a cleaning solvent to save
the ozone layer. Folks banned one of the most effective electronic cleaning
solvents, but at the same time did not ban cattle "flatulence" which is my
understanding that this deletes more ozone that all the Freon did (so some
folks say). It is my understanding that banning Freon type materials also
contributed to more tiles falling off the space shuttle due to NASA desire
to be environmentally responsible.
What we need is an international policy similar to what IPC preaches. That
is, don't create a requirement unless it can be backed up by data. Where is
the science data that shows if we delete the miniscule amount of lead from
electronic soldering we will save the environment?
I am all in favor of saving the environment where this makes sense and can
be done in an economical manner and is the right technical thing to do. But
this elimination of lead from solder will do little to save the environment.
----- Original Message -----
From: Joe Fjelstad<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Friday, April 28, 2006 11:27 AM
Subject: Re: [TN] NTC Thank you for all of your support for Pushback
Thanks Ramon.
Looks like some of those in the media are gaining interest in depth over
demagogy.
"NASA safety studies show that an inadvertent thruster firing could tear
apart the station and a docked shuttle, triggering rapid
depressurization of both spacecraft and killing all aboard"
No problem there for the members of the EU Parliament ... only a problem
if
you are on one of the two craft :-(
As was noted earlier, this misguided mandate called RoHS (but mostly
tagged
lead-free for marketing purposes) is poised to extend its reach and
possibly
(likely?) negative reliability effects beyond intentions, simply because
of
the confusion and arbitrariness of the choices.
Small examples...Why 0.1% Pb for electronics when the EPA allows 0.2% for
water pipe solders? Why WEEE and then RoHS, WEEE should obviate RoHS
(certainly
seems very true for lead)
John rightfully pointed out that the EU parliament appears to be a
bureaucracy without a country. I would add that it appears also to have
authority
without responsibility.
And so it goes...
Joe
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to
[log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentp
age.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori
at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|